Physical Properties | Original Value | Comments |
|
Density | 50 lb/ft³ | ASTM D1505 |
Specific Gravity | 1.25 g/cc | ASTM D792 |
Mechanical Properties |
|
Hardness, Shore D | 82 | Instantaneous; ASTM D2240 |
Tensile Strength, Yield | 7620 psi | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
Tensile Modulus | 400000 psi | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
Flexural Modulus | 370 ksi | ASTM D790 |
Flexural Strength | 12800 psi | ASTM D790 |
Thermal Properties |
|
Deflection Temperature at 0.46 MPa (66 psi) | 183 °F | Unannealed, 0.125 in bars; ASTM D648 |
Optical Properties |
|
Transmission, Visible | 78 % | 20.0 mils, 400 nm |
Transmission, Visible | 84 % | 20.0 mils, 700 nm |
Processing Properties |
|
Melt Temperature | 390 - 415 °F | Blow Molding |
Descriptive Properties | |
Product Form | Pellets | |
|