PolyOne Geon® 78812 Vinyl Compound - Flexible (FPVC)

Return to last searchReturn to last search
Printer friendly version Printer friendly versionAdd to Folder:
Excel Download Download to Excel (requires Excel and Windows)
 Export data to your CAD/FEA program

Subcategory: Polymer; Thermoplastic; Vinyl

Material Notes:

Description/Features:

  • Medium Gloss

Applications:

  • General Purpose

Market:

  • Automotive

Processing Method:

  • Extrusion and Molding

Disclaimer: Note: Automotive OEM approval(s).

Information provided by PolyOne Corporation.

Physical PropertiesOriginal ValueComments
Specific Gravity1.24 g/cc ASTM D792

Mechanical Properties
Hardness, Shore A58 15 sec; ASTM D2240
Hardness, Shore A63 Instantaneous; ASTM D2240
Tensile Strength, Ultimate1650 psi Type 4 - Flexibles, 20 in/min; ASTM D638
Tensile Strength, Ultimate600 psi Type 4 - Flexibles, 2 in/min, 100% in/in; ASTM D638
Elongation at Break400 % Type 4 - Flexibles, 20 in/min; ASTM D638
Tear Strength180 pli Die C (graves), 20 in/min; ASTM D624
Clash Berg Modulus4500 psi -31°F (-35°C); ASTM D1043

Thermal Properties
Brittleness Temperature-49 °F ASTM D746
Clash Berg Stiffness Temperature-49 °F 45,000 psi; ASTM D1043

Processing Properties
Melt Temperature335 - 350 °F Extrusion

Descriptive Properties
Automotive ApprovalDaimlerChrysler, MS-DC225 
Product FormPellets 
Printer friendly version Printer friendly version


Instant Quotes for Quick Parts!Upload your 3D CAD model, select process, quantity, material, and instantly receive your unique, binding quote.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。