PolyOne Geon® 78815 Vinyl Compound - Flexible (FPVC)
Subcategory: Polymer; Thermoplastic; Vinyl
Material Notes:
Description/Features: Applications: Market: Processing Method: Disclaimer: Note: Automotive OEM approval(s). Information provided by PolyOne Corporation.
Physical Properties | Original Value | Comments |
|
Specific Gravity | 1.34 g/cc | ASTM D792 |
Mechanical Properties |
|
Hardness, Shore A | 86 | 15 sec; ASTM D2240 |
Tensile Strength, Ultimate | 2799 psi | 20 in/min; ASTM D638 |
Elongation at Break | 290 % | 20 in/min; ASTM D638 |
Tear Strength | 450 pli | Die C (graves), 2 in/min; ASTM D1004 |
Processing Properties |
|
Melt Temperature | 360 - 375 °F | Extrusion |
Descriptive Properties | |
Automotive Approval | DaimlerChrysler, MS-DC228 | |
Product Form | Pellets | |
|
Printer friendly version |
|