PolyOne Geon® 85889 Vinyl Compound - Rigid (RPVC)
Subcategory: Polymer; Thermoplastic; Vinyl
Material Notes:
Description/Features: - Exterior-Weatherable
- High Flow
- High Gloss
Applications: - Custom Profiles
- Greenhouse Trim
Market: Processing Method: Disclaimer: Note: Automotive OEM approval(s). Note: The Cell Classification was determined using the notched Izod test with injection molded samples. Information provided by PolyOne Corporation.
| Physical Properties | Original Value | Comments |
|
| Specific Gravity | 1.36 g/cc | ASTM D792 |
Mechanical Properties |
|
| Hardness, Shore D | 81.9 | 15 sec; ASTM D2240 |
| Tensile Strength, Yield | 6470 psi | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
| Tensile Modulus | 362600 psi | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
| Flexural Modulus | 369 ksi | ASTM D790 |
| Flexural Strength | 10860 psi | ASTM D790 |
| Dart Drop Total Energy | 0.13 ft-lb/mil | Procedure A, 0.125 in Conical Dart, 73°F (23°C); ASTM D4226 |
| Dart Drop Total Energy | 0.29 ft-lb/mil | Procedure B, 0.125 in Conical Dart, 73°F (23°C); ASTM D4226 |
| Izod Impact, Notched | 16 ft-lb/in | Method A, Injection Molded, 0.125 in bars, 73°F (23°C); ASTM D256 |
| Izod Impact, Notched | 4.2 ft-lb/in | Method A, With Grain - Comp. Molded, 0.125 in bars, 73°F (23°C); ASTM D256 |
| Izod Impact, Notched | 8.7 ft-lb/in | Method A, Against Grain - Comp. Molded, 0.125 in bars, 73°F (23°C); ASTM D256 |
Thermal Properties |
|
| CTE, linear 68°F | 46 µin/in-°F | ASTM D696 |
| Deflection Temperature at 1.8 MPa (264 psi) | 163 °F | Unannealed, 0.125 in bars; ASTM D648 |
Processing Properties |
|
| Melt Temperature | 360 - 380 °F | |
Descriptive Properties | |
| Automotive Approval | General Motors, GMP 7001M PVC | |
| Cell Classification D1784 | 16344 | ASTM D1784 |
| Cell Classification D4216 | 14243233 | ASTM D4216 |
| Ease of Sizing | Acceptable | |
|