PolyOne Geon® 86155 Vinyl Compound - Flexible (FPVC)
Subcategory: Polymer; Thermoplastic; Vinyl
Material Notes:
Description/Features: Applications: Processing Method: Disclaimer: NOTE: All ingredients used in the formulation of this compound are listed in the United States FDA Code of Federal Regulations, Title 21. The only restriction is that the plasticizer is “For foods of high water content only”. This material is also listed under NSF Std. 61. This listing covers many uses and restrictions may apply depending on the application. It is the customer's responsibility to ensure that the compound is suitable for its intended application. Please contact us to review the suitability of specific products in specific applications. Information provided by PolyOne Corporation.
| Physical Properties | Original Value | Comments |
|
| Specific Gravity | 1.24 g/cc | ASTM D792 |
Mechanical Properties |
|
| Hardness, Shore A | 84 | 15 sec; ASTM D2240 |
| Hardness, Shore A | 90 | Instantaneous; ASTM D2240 |
| Tensile Strength, Ultimate | 1550 psi | Type 4 - Flexibles, 20 in/min, 100% in/in; ASTM D638 |
| Tensile Strength, Ultimate | 2650 psi | Type 4 - Flexibles, 20 in/min; ASTM D638 |
| Elongation at Break | 400 % | Type 4 - Flexibles, 20 in/min; ASTM D638 |
| Tear Strength | 435 pli | Die C (graves), 20 in/min; ASTM D624 |
Thermal Properties |
|
| Brittleness Temperature | -16.6 °F | ASTM D746 |
|
Printer friendly version |
|