PolyOne Geon® 8700A Vinyl Compound - Rigid (RPVC)
Subcategory: Polymer; Thermoplastic; Vinyl
Material Notes:
Description/Features: - Interior
- Excellent Dimensional Stability
- High Melt Strength
- UL 94 V0
- UL 94 5VA
- CSA V0
- NSF STD 51
Applications: - General Purpose
- Custom Profiles-Complex
- Custom Profiles-Thick wall
- Beltline Moldings
Market: Processing Method: PolyOne First ChoiceDisclaimer: Note: Automotive OEM approval(s). Note: NSF listings are obtained on specific colors. Contact PolyOne for the latest listing of approved colors for this product. Note: The Cell Classification was determined using the notched Izod test with injection molded samples. Information provided by PolyOne Corporation.
Physical Properties | Original Value | Comments |
|
Specific Gravity | 1.38 g/cc | ASTM D792 |
Mechanical Properties |
|
Hardness, Rockwell R | 111 | ASTM D785 |
Hardness, Shore D | 78 | 15 sec; ASTM D2240 |
Tensile Strength, Yield | 6200 psi | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
Tensile Modulus | 390000 psi | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
Flexural Modulus | 380 ksi | ASTM D790 |
Flexural Strength | 11000 psi | ASTM D790 |
Compressive Strength | 8100 psi | ASTM D695 |
Dart Drop Total Energy | 0.07 ft-lb/mil | Procedure A, 0.125 in Conical Dart, 73°F (23°C); ASTM D4226 |
Dart Drop Total Energy | 0.07 ft-lb/mil | Procedure B, 0.125 in Conical Dart, 73°F (23°C); ASTM D4226 |
Izod Impact, Notched | 1.1 ft-lb/in | Method A, Compression Molded, 0.125 in bars, 0°F (-18°C); ASTM D256 |
Izod Impact, Notched | 1.6 ft-lb/in | Method A, Compression Molded, 0.125 in bars, 32°F (0°C); ASTM D256 |
Izod Impact, Notched | 17 ft-lb/in | Method A, Compression Molded, 0.125 in bars, 73°F (23°C); ASTM D256 |
Electrical Properties |
|
Dielectric Constant | 3.3 | 1,000 Hz; ASTM D150 |
Dielectric Constant | 3.9 | 60 Hz; ASTM D150 |
Dielectric Strength | 690 V/mil | ASTM D149 |
Dissipation Factor | 0.029 | 60 Hz, 86°F (30°C), 24 hrs; ASTM D150 |
Dissipation Factor | 0.04 | 1,000 Hz, 86°F (30°C), 24 hrs; ASTM D150 |
Thermal Properties |
|
CTE, linear 68°F | 37 µin/in-°F | ASTM D696 |
Deflection Temperature at 1.8 MPa (264 psi) | 163 °F | Unannealed, 0.125 in bars; ASTM D648 |
Flammability, UL94 | V-0 | All Colors; 0.028 in. |
Flammability, UL94 | V-0 | All Colors; 0.034 in. |
Flammability, UL94 | 7 | All Colors; 0.059 in. |
Processing Properties |
|
Melt Temperature | 355 - 360 °F | Extrusion |
Descriptive Properties | |
Automotive Approval | General Motors, GMP 7001M PVC | |
Cell Classification D1784 | 16344 | ASTM D1784 |
Ease of Sizing | Excellent | |
|