PolyOne Geon® 87556 Vinyl Compound - Rigid (RPVC)
Subcategory: Polymer; Thermoplastic; Vinyl
Material Notes:
Description/Features: - Transparent
- Interior UV Stable
- High Impact
- UL 94 V0
Applications: - Custom Profiles
- Point of Purchase Datastrips
- General Purpose
Processing Method: PolyOne First ChoiceDisclaimer: Note: The Cell Classification was determined using the notched Izod test with injection molded samples. Information provided by PolyOne Corporation.
| Physical Properties | Original Value | Comments |
|
| Specific Gravity | 1.33 g/cc | ASTM D792 |
Mechanical Properties |
|
| Hardness, Shore D | 82 | 15 sec; ASTM D2240 |
| Tensile Strength, Yield | 7740 psi | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
| Tensile Modulus | 404500 psi | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
| Flexural Modulus | 412 ksi | ASTM D790 |
| Flexural Strength | 12840 psi | ASTM D790 |
| Dart Drop Total Energy | 0.1 ft-lb/mil | Procedure A, 0.125 in Conical Dart, 73°F (23°C); ASTM D4226 |
| Dart Drop Total Energy | 0.32 ft-lb/mil | Procedure B, 0.125 in Conical Dart, 73°F (23°C); ASTM D4226 |
| Izod Impact, Notched | 10.7 ft-lb/in | Method A, Against Grain - Comp. Molded, 0.125 in bars, 73°F (23°C); ASTM D256 |
| Izod Impact, Notched | 2.6 ft-lb/in | Method A, With Grain - Comp. Molded, 0.125 in bars, 73°F (23°C); ASTM D256 |
| Izod Impact, Notched | 20.5 ft-lb/in | Method A, Injection Molded, 0.125 in bars, 73°F (23°C); ASTM D256 |
Thermal Properties |
|
| CTE, linear 68°F | 39 µin/in-°F | ASTM D696 |
| Deflection Temperature at 1.8 MPa (264 psi) | 153 °F | Unannealed, 0.125 in bars; ASTM D648 |
| Flammability, UL94 | V-0 | All Colors; 0.059 in. |
Processing Properties |
|
| Melt Temperature | 360 - 380 °F | Extrusion |
Descriptive Properties | |
| Cell Classification D1784 | 16453 | ASTM D1784 |
|
Printer friendly version |
|