PolyOne Geon® 87624 Vinyl Compound - Rigid (RPVC)

Return to last searchReturn to last search
Printer friendly version Printer friendly versionAdd to Folder:
Excel Download Download to Excel (requires Excel and Windows)
 Export data to your CAD/FEA program

Subcategory: Polymer; Thermoplastic; Vinyl

Material Notes:

Description/Features:

  • Interior UV Stable
  • Pearlescent Appearance
  • Dark Colors

Applications:

  • Custom Profiles
  • Capstock
  • Vertical Blinds

Processing Method:

  • CoExtrusion
PolyOne First Choice

Information provided by PolyOne Corporation.

Physical PropertiesOriginal ValueComments
Specific Gravity1.39 g/cc ASTM D792

Mechanical Properties
Hardness, Shore D84 15 sec; ASTM D2240
Tensile Strength, Yield7000 psi Type 1 - Rigids, 0.2 in/min; ASTM D638
Tensile Modulus400000 psi Type 1 - Rigids, 0.2 in/min; ASTM D638
Flexural Modulus500 ksi ASTM D790
Flexural Strength13000 psi ASTM D790
Dart Drop Total Energy0.09 ft-lb/mil Procedure A, 0.125 in Conical Dart, 73°F (23°C); ASTM D4226
Dart Drop Total Energy0.17 ft-lb/mil Procedure B, 0.125 in Conical Dart, 73°F (23°C); ASTM D4226
Izod Impact, Notched0.6 ft-lb/in Method A, With Grain - Comp. Molded, 0.125 in bars, 73°F (23°C); ASTM D256
Izod Impact, Notched0.6 ft-lb/in Method A, Against Grain - Comp. Molded, 0.125 in bars, 73°F (23°C); ASTM D256

Thermal Properties
CTE, linear 68°F36 µin/in-°F ASTM D696
Deflection Temperature at 1.8 MPa (264 psi)149 °F Unannealed, 0.125 in bars; ASTM D648

Processing Properties
Melt Temperature360 - 390 °F Extrusion
Printer friendly version Printer friendly version


Instant Quotes for Quick Parts!Upload your 3D CAD model, select process, quantity, material, and instantly receive your unique, binding quote.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。