Physical Properties | Original Value | Comments |
|
Specific Gravity | 1.38 g/cc | ASTM D792 |
Mechanical Properties |
|
Hardness, Shore D | 84.6 | 15 sec; ASTM D2240 |
Tensile Strength, Yield | 8250 psi | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
Tensile Modulus | 415600 psi | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
Flexural Modulus | 423 ksi | ASTM D790 |
Flexural Strength | 13560 psi | ASTM D790 |
Dart Drop Total Energy | 0.12 ft-lb/mil | Procedure A, 0.125 in Conical Dart, 73°F (23°C); ASTM D4226 |
Dart Drop Total Energy | 0.33 ft-lb/mil | Procedure B, 0.125 in Conical Dart, 73°F (23°C); ASTM D4226 |
Izod Impact, Notched | 0.3 ft-lb/in | Method A, With Grain - Comp. Molded, 0.125 in bars, 73°F (23°C); ASTM D256 |
Izod Impact, Notched | 0.65 ft-lb/in | Method A, Against Grain - Comp. Molded, 0.125 in bars, 73°F (23°C); ASTM D256 |
Izod Impact, Notched | 3.9 ft-lb/in | Method A, Injection Molded, 0.125 in bars, 73°F (23°C); ASTM D256 |
Thermal Properties |
|
CTE, linear 68°F | 39 µin/in-°F | ASTM D696 |
Deflection Temperature at 1.8 MPa (264 psi) | 142 °F | Unannealed, 0.125 in bars; ASTM D648 |
Flammability, UL94 | V-0 | Transparent; 0.059 in. |
Processing Properties |
|
Melt Temperature | 360 - 380 °F | Extrusion |
Descriptive Properties | |
Cell Classification D1784 | 11553 | ASTM D1784 |
|