PolyOne Geon® 87727-0284 Vinyl Compound - Rigid (RPVC)

Return to last searchReturn to last search
Printer friendly version Printer friendly versionAdd to Folder:
Excel Download Download to Excel (requires Excel and Windows)
 Export data to your CAD/FEA program

Subcategory: Polymer; Thermoplastic; Vinyl

Material Notes:

Description/Features:

  • Interior UV Stable
  • Pearlescent Appearance
  • Translucent
  • Colorless

Applications:

  • Custom Profiles
  • Capstock
  • Vertical Blinds

Processing Method:

  • Extrusion-Single Screw

Physical property testing was based on the Geon® 87727 Trans 0020.
PolyOne First Choice

Disclaimer: Note: The Cell Classification was determined using the notched Izod test with injection molded samples.

Information provided by PolyOne Corporation.

Physical PropertiesOriginal ValueComments
Specific Gravity1.38 g/cc ASTM D792

Mechanical Properties
Hardness, Shore D84.6 15 sec; ASTM D2240
Tensile Strength, Yield8250 psi Type 1 - Rigids, 0.2 in/min; ASTM D638
Tensile Modulus415600 psi Type 1 - Rigids, 0.2 in/min; ASTM D638
Flexural Modulus423 ksi ASTM D790
Flexural Strength13560 psi ASTM D790
Dart Drop Total Energy0.12 ft-lb/mil Procedure A, 0.125 in Conical Dart, 73°F (23°C); ASTM D4226
Dart Drop Total Energy0.33 ft-lb/mil Procedure B, 0.125 in Conical Dart, 73°F (23°C); ASTM D4226
Izod Impact, Notched0.3 ft-lb/in Method A, With Grain - Comp. Molded, 0.125 in bars, 73°F (23°C); ASTM D256
Izod Impact, Notched0.65 ft-lb/in Method A, Against Grain - Comp. Molded, 0.125 in bars, 73°F (23°C); ASTM D256
Izod Impact, Notched3.9 ft-lb/in Method A, Injection Molded, 0.125 in bars, 73°F (23°C); ASTM D256

Thermal Properties
CTE, linear 68°F39 µin/in-°F ASTM D696
Deflection Temperature at 1.8 MPa (264 psi)142 °F Unannealed, 0.125 in bars; ASTM D648
Flammability, UL94V-0 Transparent; 0.059 in.

Processing Properties
Melt Temperature360 - 380 °F Extrusion

Descriptive Properties
Cell Classification D178411553 ASTM D1784
Printer friendly version Printer friendly version


Instant Quotes for Quick Parts!Upload your 3D CAD model, select process, quantity, material, and instantly receive your unique, binding quote.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。