PolyOne Geon® 90049 Vinyl Compound - Flexible (FPVC)
Subcategory: Polymer; Thermoplastic; Vinyl
Material Notes:
Description/Features: - Exterior
- High Gloss
- Transparent
Applications: Market: Processing Method: PolyOne First ChoiceDisclaimer: Note: Automotive OEM approval(s). Information provided by PolyOne Corporation.
| Physical Properties | Original Value | Comments |
|
| Specific Gravity | 1.22 g/cc | ASTM D792 |
| Collected Volatile Condensable Material | 0.43 % | Emery, 221°F (105°C), 0.075 in; ASTM D1203B |
Mechanical Properties |
|
| Hardness, Shore A | 83 | 15 sec; ASTM D2240 |
| Tensile Strength, Ultimate | 2785 psi | Type 4 - Flexibles, 20 in/min; ASTM D638 |
| Elongation at Break | 324 % | Type 4 - Flexibles, 20 in/min; ASTM D638 |
| Tear Strength | 361 pli | Die C (graves), 2 in/min; ASTM D1004 |
Descriptive Properties | |
| Automotive Approval | General Motors, GMP.PVC.010 | Pass |
| Automotive Approval | DaimlerChrysler, MS-DC211-B | Pass |
| Fungal Resistance | Pass | ASTM G21 |
| Low Temperature Flexibility (LTF) | Pass | 12 mm, -20°F (-29°C), 4 hrs, 0.020 in |
| Product Form | Pellets | |
| Xenon Weatherometer - Exterior | Pass | 2,500 kJ/m², Natural, dE*; SAE J1960 |
|
Printer friendly version |
|