PolyOne Geon® 90072 Vinyl Compound - Flexible (FPVC)
Subcategory: Polymer; Thermoplastic; Vinyl
Material Notes:
Description/Features: Market: Processing Method: PolyOne First ChoiceInformation provided by PolyOne Corporation.
| Physical Properties | Original Value | Comments |
|
| Specific Gravity | 1.26 g/cc | ASTM D792 |
Mechanical Properties |
|
| Hardness, Shore A | 88 | 15 sec; ASTM D2240 |
| Tensile Strength, Ultimate | 2828 psi | Type 4 - Flexibles, 20 in/min; ASTM D638 |
| Elongation at Break | 260 % | Type 4 - Flexibles, 20 in/min; ASTM D638 |
| Tear Strength | 500 pli | Die C (graves), 2 in/min; ASTM D1004 |
Thermal Properties |
|
| Brittleness Temperature | -18.4 °F | ASTM D746 |
Processing Properties |
|
| Melt Temperature | 350 - 370 °F | |
Descriptive Properties | |
| Automotive Approval | Aftermarket Only, None | |
| Product Form | Pellets | |
|