PolyOne Geon® 90201 Vinyl Compound - Flexible (FPVC)

Return to last searchReturn to last search
Printer friendly version Printer friendly versionAdd to Folder:
Excel Download Download to Excel (requires Excel and Windows)
 Export data to your CAD/FEA program

Subcategory: Polymer; Thermoplastic; Vinyl

Material Notes:

Description/Features:

  • Exterior

Applications:

  • Window Encapsulation
  • Greenhouse Trim

Market:

  • Automotive

Processing Method:

  • Extrusion
  • Injection Molding

Information provided by PolyOne Corporation.

Physical PropertiesOriginal ValueComments
Specific Gravity1.27 g/cc ASTM D792
Collected Volatile Condensable Material0.75 % Method A, 221°F (105°C), 0.075 in; ASTM D1203B

Mechanical Properties
Hardness, Shore A74 15 sec; ASTM D2240
Tensile Strength, Ultimate1885 psi Type 4 - Flexibles, 20 in/min; ASTM D638
Elongation at Break340 % Type 4 - Flexibles, 20 in/min; ASTM D638
Tear Strength271 pli Die C (graves), 2 in/min; ASTM D1004

Descriptive Properties
Automotive ApprovalGeneral Motors, GMP.PVC.009 Pass
Fungal ResistancePass ASTM G21
Low Temperature Flexibility (LTF)Pass 12 mm, -20°F (-29°C), 4 hrs, 0.020 in
Product FormPellets 
Xenon Weatherometer - ExteriorPass 2,500 kJ/m², Black, dE*; SAE J1960
Printer friendly version Printer friendly version


Instant Quotes for Quick Parts!Upload your 3D CAD model, select process, quantity, material, and instantly receive your unique, binding quote.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。