PolyOne Geon® 90209 Vinyl Compound - Flexible (FPVC)
Subcategory: Polymer; Thermoplastic; Vinyl
Material Notes:
Description/Features: Applications: - Seat Welting
- Protective Sleeves
Market: Processing Method: Information provided by PolyOne Corporation.
Physical Properties | Original Value | Comments |
|
Specific Gravity | 1.37 g/cc | ASTM D792 |
Mechanical Properties |
|
Hardness, Shore A | 74 | 15 sec; ASTM D2240 |
Hardness, Shore A | 80 | Instantaneous; ASTM D2240 |
Tensile Strength, Ultimate | 2176 psi | Type 4 - Flexibles, 20 in/min; ASTM D638 |
Elongation at Break | 325 % | Type 4 - Flexibles, 20 in/min; ASTM D638 |
Tear Strength | 343 pli | Die C (graves), 2 in/min; ASTM D1004 |
Thermal Properties |
|
Brittleness Temperature | -29.2 °F | ASTM D746 |
Descriptive Properties | |
Product Form | Pellets | |
|
Printer friendly version |
|