PolyOne Geon® 90401 Vinyl Alloy - Flexible (FPVC alloy)
Subcategory: Polymer; Thermoplastic; Vinyl
Material Notes:
Description/Features: Applications: Market: Processing Method: Disclaimer: Note: Automotive OEM approval(s). Information provided by PolyOne Corporation.
Physical Properties | Original Value | Comments |
|
Specific Gravity | 1.24 g/cc | ASTM D792 |
Mechanical Properties |
|
Hardness, Shore A | 75 | 15 sec; ASTM D2240 |
Tensile Strength, Ultimate | 2060 psi | Type 4 - Flexibles, 20 in/min; ASTM D638 |
Elongation at Break | 313 % | Type 4 - Flexibles, 20 in/min; ASTM D638 |
Tear Strength | 206 pli | Die C (graves), 20 in/min; ASTM D624 |
Thermal Properties |
|
Flammability Test | 0 | in/min; FMVSS 302 |
Optical Properties |
|
Gloss | 3.5 % | 60º Gardner; ASTM D523 |
Descriptive Properties | |
Automotive Approval | General Motors, GMP.PVC.077 | |
Cold Flexibility | Pass | -20°F (-29°C), 25 mm, 4 hrs, 0.075 in; GM9503P |
Fogging | 86 % | 3 hrs, 212°F (100°C), 70°F (21°C), after 1 hour; SAE J1756 |
Product Form | Pellets | |
Xenon Weatherometer - Interior | Pass | 1,240 kJ/m², All Colors, dE*; SAE J1885 |
|