PolyOne Geon® 90451 Vinyl Compound - Flexible (FPVC)
Subcategory: Polymer; Thermoplastic; Vinyl
Material Notes:
Description/Features: Applications: Market: Processing Method: Disclaimer: Note: Automotive OEM approval(s). Information provided by PolyOne Corporation.
| Physical Properties | Original Value | Comments |
|
| Specific Gravity | 1.29 g/cc | ASTM D792 |
Mechanical Properties |
|
| Hardness, Shore A | 72 | 15 sec; ASTM D2240 |
| Tensile Strength, Ultimate | 1940 psi | Type 4 - Flexibles, 20 in/min; ASTM D638 |
| Elongation at Break | 345 % | Type 4 - Flexibles, 20 in/min; ASTM D638 |
| Tear Strength | 320 pli | Die C (graves), 20 in/min; ASTM D624 |
Thermal Properties |
|
| Brittleness Temperature | -29.2 °F | ASTM D746 |
| Flammability Test | 0 | in/min; FMVSS 302 |
Descriptive Properties | |
| Automotive Approval | Subaru, None | |
| Cold Flexibility | Pass | -20°F (-29°C), 25 mm, 4 hrs, 0.075 in; GM9503P |
| Fogging | 90 % | 3 hrs, 212°F (100°C), 70°F (21°C), after 1 hour; SAE J1756 |
| Fogging | 88 % | 6 hrs, 203°F (95°C), 100°F (38°C), after 16 hours; SAE J1756 |
| Product Form | Pellets | |
| Xenon Weatherometer - Interior | Pass | 602 kj/m², All Colors, dE*; SAE J1885 |
|
Printer friendly version |
|