MatWeb - Material Property Data 用 MatWeb 登广告!    Register Now
越过59,000 以上, 金属、塑料、陶瓷和合成物的数据资料库。
MatWeb - Material Property Data 主页  •  搜寻  •  工具  •  供应商  •  文件夹  •  有关我们  •  常用问题  •  登录   •  English English English 
  搜寻方法:  高级先进 | 材料类型 | 特性 | 构成份  | 商标  | 制造商
    Search

COMSOL CD

Degussa AG VESTAMID® L1640 nf (dry properties) Nylon 12

Return to last searchReturn to last search
Printer friendly version Printer friendly versionAdd to Folder:
Excel Download Download to Excel (requires Excel and Windows)
 Export data to your CAD/FEA program

Subcategory: Nylon; Nylon 12; Polymer; Thermoplastic

Close Analogs: This former Creanova product line is a part of Degussa AG as of 2001. This grade is not part of the current Degussa product line.

Key Words: Polyamide

Material Notes:
ISO data as provided by the manufacturer, Creanova, Inc.

Uses: Wire insulation, fiber optics jacketing.

No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.

Physical PropertiesOriginal ValueComments
Density1.01 g/cc 
Water Absorption1 % 
Moisture Absorption at EquilibriumMax 0.5 % Humidity Absorption
Melt Flow60 g/10 min 

Mechanical Properties
Tensile Strength, Yield48 MPa 
Elongation at BreakMin 50 % 
Elongation at Yield6 % 
Modulus of Elasticity1.5 GPa 
Charpy Impact UnnotchedNB 
Charpy Impact, Notched, Low Temp0.6 J/cm² at -30°C
Charpy Impact, Unnotched Low TempNB at -30°C
Charpy Impact, Notched0.5 J/cm² 
Tensile Creep Modulus, 1 hour900 MPa 
Tensile Creep Modulus, 1000 hours470 MPa 

Electrical Properties
Electrical ResistivityMin 1e+015 ohm-cm 
Surface ResistanceMin 1e+015 ohm 
Dielectric Constant2 at 1 MHz.
Dielectric Constant, Low Frequency3 100 Hz
Dielectric Strength27 kV/mm 
Dissipation Factor0.028 at 1 MHz.
Dissipation Factor, Low Frequency0.04 100 Hz
Comparative Tracking Index600 V 

Thermal Properties
CTE, linear 20°C100 µm/m-°C in flow direction.
CTE, linear 20°C Transverse to Flow100 µm/m-°C 
Deflection Temperature at 0.46 MPa (66 psi)120 °C 
Deflection Temperature at 1.8 MPa (264 psi)50 °C 
Vicat Softening Point140 °C 50°C/hr/50 N
UL RTI, Electrical110 °C 
UL RTI, Mechanical with Impact70 °C 
UL RTI, Mechanical without Impact95 °C 
Flammability, UL94HB 1.6 mm
Flammability, UL94HB 3.2 mm
Printer friendly version Printer friendly version


New MatWeb Services

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。