Degussa AG VESTAMID® L2123 sw 9.7507 (as-conditioned) Nylon 12
Subcategory: Nylon; Nylon 12; Polymer; Thermoplastic
Close Analogs: This former Creanova product line is a part of Degussa AG as of 2001.
Key Words: Polyamide
Material Notes: ISO data as provided by the manufacturer, Creanova, Inc. Uses: Flexible tubing for the automobile industry.
No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
| Physical Properties | Original Value | Comments |
|
| Density | 1.03 g/cc | |
| Moisture Absorption at Equilibrium | Max 0.5 % | Humidity Absorption |
Mechanical Properties |
|
| Tensile Strength, Yield | 25 MPa | |
| Elongation at Break | Min 50 % | |
| Elongation at Yield | 30 % | |
| Modulus of Elasticity | 0.4 GPa | |
| Charpy Impact Unnotched | NB | |
| Charpy Impact, Notched, Low Temp | 0.8 J/cm² | at -30°C |
| Charpy Impact, Unnotched Low Temp | NB | at -30°C |
| Charpy Impact, Notched | NB | |
Electrical Properties |
|
| Electrical Resistivity | 7e+010 ohm-cm | |
| Surface Resistance | 2e+012 ohm | |
| Dielectric Constant | 4 | at 1 MHz. |
| Dielectric Constant, Low Frequency | 15 | 100 Hz |
| Dielectric Strength | 33 kV/mm | |
| Dissipation Factor | 0.14 | at 1 MHz. |
| Dissipation Factor, Low Frequency | 0.33 | 100 Hz |
Thermal Properties |
|
| CTE, linear 20°C | Max 50 µm/m-°C | |
| Deflection Temperature at 0.46 MPa (66 psi) | 90 °C | |
| Deflection Temperature at 1.8 MPa (264 psi) | 45 °C | |
| Vicat Softening Point | 120 °C | 50°C/hr/50 N |
|