Degussa AG VESTAMID® X4442 nf (dry properties) Polyether Block Amide (PEBA)
Subcategory: Elastomer, TPE; Polyether Block Amide (PEBA); Polymer; Thermoplastic
Close Analogs: This former Creanova product line is a part of Degussa AG as of 2001.
Key Words: Polyamide
Material Notes: ISO data as provided by the manufacturer, Creanova, Inc. Uses: Sport articles.
No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
Physical Properties | Original Value | Comments |
|
Density | 1.01 g/cc | |
Mechanical Properties |
|
Hardness, Shore D | 66 | |
Tensile Strength, Yield | 27 MPa | |
Elongation at Break | Min 50 % | |
Elongation at Yield | 25 % | |
Modulus of Elasticity | 0.53 GPa | |
Charpy Impact Unnotched | NB | |
Charpy Impact, Notched, Low Temp | 0.9 J/cm² | at -30°C |
Charpy Impact, Unnotched Low Temp | NB | at -30°C |
Charpy Impact, Notched | NB | |
Electrical Properties |
|
Electrical Resistivity | 7e+012 ohm-cm | |
Dielectric Constant | 4 | at 1 MHz. |
Dielectric Constant, Low Frequency | 9 | 100 Hz |
Dielectric Strength | 32 kV/mm | |
Dissipation Factor | 0.11 | at 1 MHz. |
Dissipation Factor, Low Frequency | 0.14 | 100 Hz |
Comparative Tracking Index | 600 V | |
Thermal Properties |
|
CTE, linear 20°C | 100 µm/m-°C | in flow direction. |
CTE, linear 20°C Transverse to Flow | 100 µm/m-°C | |
Deflection Temperature at 0.46 MPa (66 psi) | 100 °C | |
Deflection Temperature at 1.8 MPa (264 psi) | 45 °C | |
Vicat Softening Point | 130 °C | 50°C/hr/50 N |
Flammability, UL94 | HB | 1.6 mm |
|