Degussa AG VESTAMID® X7324 nf (dry properties) Nylon 12
Subcategory: Nylon; Nylon 12; Polymer; Thermoplastic
Close Analogs: This former Creanova product line is a part of Degussa AG as of 2001. This grade is not part of the current Degussa product line.
Key Words: Polyamide
Material Notes: ISO data as provided by the manufacturer, Creanova, Inc. Uses: Bearing housing for windshield wipers.
| Physical Properties | Original Value | Comments |
|
| Density | 1.24 g/cc | |
| Water Absorption | 1 % | |
| Moisture Absorption at Equilibrium | Max 0.5 % | Humidity Absorption |
Mechanical Properties |
|
| Tensile Strength, Yield | 69 MPa | |
| Elongation at Break | 12 % | |
| Elongation at Yield | 4 % | |
| Modulus of Elasticity | 4 GPa | |
| Charpy Impact Unnotched | 7 J/cm² | |
| Charpy Impact, Notched, Low Temp | 1.1 J/cm² | at -30°C |
| Charpy Impact, Unnotched Low Temp | 6.5 J/cm² | at -30°C |
| Charpy Impact, Notched | 1 J/cm² | |
Electrical Properties |
|
| Electrical Resistivity | 5e+014 ohm-cm | |
| Surface Resistance | Min 1e+015 ohm | |
| Dielectric Constant | 4 | at 1 MHz. |
| Dielectric Constant, Low Frequency | 4 | 100 Hz |
| Dissipation Factor | 0.0042 | at 1 MHz. |
| Dissipation Factor, Low Frequency | 0.065 | 100 Hz |
| Comparative Tracking Index | 600 V | |
Thermal Properties |
|
| CTE, linear 20°C | Max 50 µm/m-°C | Parallel direction |
| CTE, linear 20°C Transverse to Flow | Max 50 µm/m-°C | |
| Deflection Temperature at 0.46 MPa (66 psi) | 170 °C | |
| Deflection Temperature at 1.8 MPa (264 psi) | 130 °C | |
| Vicat Softening Point | 170 °C | 50°C/hr/50 N |
| Flammability, UL94 | HB | 1.6 mm |
| Flammability, UL94 | HB | 3.2 mm |
|