COMSOL CD

Degussa AG Vestamid® D18 Nylon 612 (Conditioned)

Return to last searchReturn to last search
Printer friendly version Printer friendly versionAdd to Folder:
Excel Download Download to Excel (requires Excel and Windows)
 Export data to your CAD/FEA program

Subcategory: Nylon; Nylon 612; Polymer; Thermoplastic

Key Words: PA612, LN, 14-020

Material Notes:
Description: medium-viscosity base product

Applications: monofilaments, bristles with high recovery for paint brushes and tooth brushes

Information provided by degussa.

No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.

Physical PropertiesOriginal ValueComments
Density1.06 g/cc ISO 1183

Mechanical Properties
Tensile Strength, Yield52 MPa ISO 527-2/1A
Elongation at BreakMin 50 % ISO 527-2/1A
Elongation at Yield20 % ISO 527-2/1A
Tensile Modulus1.7 GPa ISO 527-2/1A
Charpy Impact UnnotchedNB 23°C; ISO 179/1eU
Charpy Impact, Notched, Low Temp0.7 J/cm² -30°C; ISO 179/1eA
Charpy Impact, Unnotched Low TempNB -30°C; ISO 179/1eU
Charpy Impact, Notched0.9 J/cm² 23°C; ISO 179/1eA

Thermal Properties
Melting Point215 °C Peak Temperature; ISO 3146, ISO 11357
Deflection Temperature at 0.46 MPa (66 psi)170 °C When conditioned at 180°C for 1 hour; ISO 75
Deflection Temperature at 1.8 MPa (264 psi)55 °C ISO 75
Deflection Temperature at 1.8 MPa (264 psi)75 °C When conditioned at 180°C for 1 hour; ISO 75
Vicat Softening Point180 °C 50N; ISO 306
Flammability, UL94HB 3.2 mm
Flammability, UL94HB 1.6 mm

Descriptive Properties
Electrolytic CorrosionA1 Step IEC 60426
Printer friendly version Printer friendly version


New MatWeb Services

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。