COMSOL CD

Degussa AG Vestamid® D18 Nylon 612 (Dry as Molded)

Return to last searchReturn to last search
Printer friendly version Printer friendly versionAdd to Folder:
Excel Download Download to Excel (requires Excel and Windows)
 Export data to your CAD/FEA program

Subcategory: Nylon; Nylon 612; Polymer; Thermoplastic

Key Words: PA612, LN, 14-020

Material Notes:
Description: medium-viscosity base product

Applications: monofilaments, bristles with high recovery for paint brushes and tooth brushes

Information provided by degussa.

Physical PropertiesOriginal ValueComments
Density1.06 g/cc ISO 1183
Moisture Absorption at Equilibrium1 % 23°C/50% R.H.; ISO 62
Water Absorption at Saturation2.7 % ISO 62
Linear Mold Shrinkage0.013 cm/cm 127x12.7x3.2 mm (processing cond. acc. To ISO 1874-2)
Linear Mold Shrinkage, Transverse0.011 cm/cm 127x12.7x3.2 mm (processing cond. acc. To ISO 1874-2)

Mechanical Properties
Tensile Strength, Yield58 MPa ISO 527-2/1A
Elongation at BreakMin 50 % ISO 527-2/1A
Elongation at Yield4 % ISO 527-2/1A
Tensile Modulus2.1 GPa ISO 527-2/1A
Charpy Impact UnnotchedNB 23°C; ISO 179/1eU
Charpy Impact, Notched, Low Temp0.6 J/cm² -30°C; ISO 179/1eA
Charpy Impact, Unnotched Low TempNB -30°C; ISO 179/1eU
Charpy Impact, Notched0.7 J/cm² 23°C; ISO 179/1eA

Electrical Properties
Dielectric Constant3.4 23°C/1 MHz; IEC 60250
Dielectric Constant, Low Frequency3.8 23°C/100 Hz; IEC 60250
Dielectric Strength28 kV/mm K20/P50; IEC 60243-1
Dissipation Factor0.031 23°C/1 MHz; IEC 60250
Dissipation Factor, Low Frequency0.026 23°C/100 Hz; IEC 60250
Comparative Tracking IndexMin 600 V Test Solution A, 100 drops; IEC 60112

Thermal Properties
CTE, linear 20°C130 µm/m-°C 23-55°C ; ISO 11359
Melting Point215 °C Peak Temperature; ISO 3146, ISO 11357
Deflection Temperature at 0.46 MPa (66 psi)140 °C ISO 75
Deflection Temperature at 1.8 MPa (264 psi)60 °C ISO 75
Deflection Temperature at 1.8 MPa (264 psi)75 °C When conditioned at 180°C for 1 hour; ISO 75
Vicat Softening Point180 °C 50N; ISO 306
Flammability, UL94HB 3.2 mm
Flammability, UL94HB 1.6 mm

Descriptive Properties
Electrolytic CorrosionA1 Step IEC 60426
Printer friendly version Printer friendly version


Instant Quotes for Quick Parts!Upload your 3D CAD model, select process, quantity, material, and instantly receive your unique, binding quote.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。