Degussa AG Vestamid® DX9320 Black 10% Glass Reinforced Nylon 612 (Conditioned)
Subcategory: Filled/Reinforced Thermoplastic; Nylon; Nylon 612; Polymer; Thermoplastic
Key Words: PA612-HI, MH, 14-040, GF10
Material Notes: Description: impact-resistant, 10% glass fiber reinforced, medium-viscosity, heat-stabilized Applications: housings subject to impact, coverings with molded-on elastomer seals Information provided by degussa.
No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
| Physical Properties | Original Value | Comments |
|
| Density | 1.12 g/cc | ISO 1183 |
Mechanical Properties |
|
| Tensile Strength at Break | 62 MPa | ISO 527-2/1A |
| Tensile Strength, Yield | 67 MPa | ISO 527-2/1A |
| Elongation at Break | 12 % | ISO 527-2/1A |
| Elongation at Yield | 5 % | ISO 527-2/1A |
| Tensile Modulus | 3.1 GPa | ISO 527-2/1A |
| Charpy Impact Unnotched | 8.5 J/cm² | 23°C; ISO 179/1eU |
| Charpy Impact, Notched, Low Temp | 0.5 J/cm² | -30°C; ISO 179/1eA |
| Charpy Impact, Unnotched Low Temp | 8.4 J/cm² | -30°C; ISO 179/1eU |
| Charpy Impact, Notched | 1.2 J/cm² | 23°C; ISO 179/1eA |
Thermal Properties |
|
| Melting Point | 215 °C | Peak Temperature; ISO 11357 |
| Deflection Temperature at 0.46 MPa (66 psi) | 201 °C | ISO 75 |
| Deflection Temperature at 1.8 MPa (264 psi) | 183 °C | ISO 75 |
| Vicat Softening Point | 199 °C | 50N; ISO 306 |
| Flammability, UL94 | HB | 1.6 mm |
|