Degussa AG Vestamid® E50-R2 Heat & Light Stabilized Nylon 12/PEBA Elastomer

Return to last searchReturn to last search
Printer friendly version Printer friendly versionAdd to Folder:
Excel Download Download to Excel (requires Excel and Windows)
 Export data to your CAD/FEA program

Subcategory: Elastomer, TPE; Nylon; Nylon 12; Polyether Block Amide (PEBA); Polymer; Thermoplastic

Material Notes:
Description: Compared to other contending thermoplastic elastomers, PA 12 elastomers are distinguished by the following properties:

  • They have low density.
  • They are highly resistant to chemicals and solvents.
  • They are easy to process and color and are easy to overmold.
  • They can be decorated easily by means of heat transfer printing.
  • They have excellent impact strength at low temperatures.
  • Their hardness and flexibility can be varied over a wide range.
  • They have high elasticity and good recovery.
  • Their mechanical properties are only slightly temperature-dependent.
  • They are free of volatile or migrating plasticizers.

Applications: permanently antistatic articles (R=102 - 105?), e.g., conveyor belts, housings, paint spray hoses

Information provided by degussa.

Physical PropertiesOriginal ValueComments
Density1.08 g/cc ISO 1183

Mechanical Properties
Hardness, Shore D50 ISO 868
Tensile Strength at Break20 MPa ISO 527-1, ISO 527-2
Elongation at BreakMin 200 % ISO 527-1, ISO 527-2
Tensile Modulus0.17 GPa ISO 527-1, ISO 527-2
50% Modulus0.013 GPa ISO 527-1, ISO 527-2
Charpy Impact UnnotchedNB 23°C; ISO 179/1eU
Charpy Impact, Notched, Low TempNB -30°C; ISO 179/1eA
Charpy Impact, Unnotched Low TempNB -30°C; ISO 179/1eU
Charpy Impact, NotchedNB 23°C; ISO 179/1eA

Electrical Properties
Volume Resistivity1000 ohm-cm Spec.; IEC 60093
Surface Resistance10000 ohm Spec.; IEC 60093

Thermal Properties
Flammability, UL94HB 1.6 mm
Printer friendly version Printer friendly version


Instant Quotes for Quick Parts!Upload your 3D CAD model, select process, quantity, material, and instantly receive your unique, binding quote.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。