Degussa AG Vestamid® E62-S3 Heat & Light Stabilized Nylon 12/PEBA Elastomer for Fiber Optic Jacketing
Subcategory: Elastomer, TPE; Nylon; Nylon 12; Polyether Block Amide (PEBA); Polymer; Thermoplastic
Material Notes: Description: E62-S3 is a PA 12 block copolymer consisting of PA 12 segments and polyether segments. The compound exhibits high flexibility and high chemical and solvent resistance. Information provided by degussa.
No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
Physical Properties | Original Value | Comments |
|
Density | 1.01 g/cc | ISO 1183 |
Water Absorption at Saturation | 1.5 % | ISO 62 |
Melt Flow | 20.2 g/10 min | 250°C/2.16 kg; ISO 1133 |
Mechanical Properties |
|
Hardness, Shore D | 62 | ISO 868 |
Tensile Strength, Yield | 24 MPa | ISO 527-2/1A |
Elongation at Break | Min 50 % | ISO 527-2/1A |
Elongation at Yield | 31 % | ISO 527-2/1A |
Tensile Modulus | 0.36 GPa | ISO 527-1/2 |
Charpy Impact Unnotched | NB | 23°C; ISO 179/1eU |
Charpy Impact, Notched, Low Temp | 0.8 J/cm² | -30°C; ISO 179/1eA |
Charpy Impact, Unnotched Low Temp | NB | -30°C; ISO 179/1eU |
Charpy Impact, Notched | 12 J/cm² | 23°C, Partial Break; ISO 179/1eA |
Thermal Properties |
|
CTE, linear 20°C | 200 µm/m-°C | 23-80°C; ISO 11359 |
Melting Point | 175 - 178 °C | DSC |
|