Degussa AG Vestamid® L1670 Nylon 12 for Fiber Optic Jacketing

Return to last searchReturn to last search
Printer friendly version Printer friendly versionAdd to Folder:
Excel Download Download to Excel (requires Excel and Windows)
 Export data to your CAD/FEA program

Subcategory: Nylon; Nylon 12; Polymer; Thermoplastic

Material Notes:
Description: L1670 is a semi-crystalline PA 12 grade of low melt viscosity; exhibiting very good flow characteristics. This grade offers consistent protection of the glass fiber against microbending and strain. Recommended for tight buffering.

Information provided by degussa.

Physical PropertiesOriginal ValueComments
Density1.01 g/cc ISO 1183
Water Absorption at Saturation1.4 % ISO 62
Melt Flow60.6 g/10 min 250°C/2.16 kg; ISO 1133

Mechanical Properties
Hardness, Shore D71 ISO 868
Tensile Strength, Yield45 MPa ISO 527-2/1A
Elongation at BreakMin 50 % ISO 527-2/1A
Elongation at Yield6 % ISO 527-2/1A
Tensile Modulus1.4 GPa ISO 527-1/2
Charpy Impact UnnotchedNB 23°C; ISO 179/1eU
Charpy Impact, Notched, Low Temp0.5 J/cm² -30°C; ISO 179/1eA
Charpy Impact, Unnotched Low TempNB -30°C; ISO 179/1eU
Charpy Impact, Notched0.4 J/cm² 23°C; ISO 179/1eA

Thermal Properties
CTE, linear 20°C150 µm/m-°C 23-80°C; ISO 11359
Melting Point175 - 178 °C DSC
Printer friendly version Printer friendly version


Instant Quotes for Quick Parts!Upload your 3D CAD model, select process, quantity, material, and instantly receive your unique, binding quote.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。