MatWeb - Material Property Data 用 MatWeb 登广告!    Register Now
越过59,000 以上, 金属、塑料、陶瓷和合成物的数据资料库。
MatWeb - Material Property Data 主页  •  搜寻  •  工具  •  供应商  •  文件夹  •  有关我们  •  常用问题  •  登录   •  English English English 
  搜寻方法:  高级先进 | 材料类型 | 特性 | 构成份  | 商标  | 制造商
    Search

COMSOL CD

Degussa AG Vestamid® X7380 23% Glass, Antistatic, Black, Electrically Conductive Nylon 12

Return to last searchReturn to last search
Printer friendly version Printer friendly versionAdd to Folder:
Excel Download Download to Excel (requires Excel and Windows)
 Export data to your CAD/FEA program

Subcategory: Nylon; Nylon 12; Polymer; Thermoplastic

Key Words: PA12-HI,MHZ,16-050,GF23

Material Notes:
Description: Medium-viscosity,23% chopped strands, heat- and light-stabilized, increased impact strength

Applications: Quick connectors in conductive fuel lines

Information provided by degussa.

No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.

Physical PropertiesOriginal ValueComments
Density1.21 g/cc ISO 1183
Moisture Absorption at Equilibrium0.6 % 23°C/50% R.H. (1mm); ISO 62
Water Absorption at Saturation1.2 % 1 mm; ISO 62
Linear Mold Shrinkage0.003 cm/cm 127x12.7x3.2 mm (processing cond. acc. To ISO 1874-2)
Linear Mold Shrinkage, Transverse0.009 cm/cm 127x12.7x3.2 mm (processing cond. acc. To ISO 1874-2)

Mechanical Properties
Tensile Strength at Break100 MPa ISO 527-1/2
Elongation at Break6 % ISO 527-1/2
Tensile Modulus5.4 GPa ISO 527-1/2
Charpy Impact Unnotched8 J/cm² 23°C; ISO 179/1eU
Charpy Impact, Notched, Low Temp0.8 J/cm² -30°C; ISO 179/1eA
Charpy Impact, Unnotched Low Temp6 J/cm² -30°C; ISO 179/1eU
Charpy Impact, Notched1.7 J/cm² 23°C; ISO 179/1eA

Electrical Properties
Volume Resistivity1e+007 ohm-cm IEC 60093
Insulation Resistance1e+007 ohm Isolation Resistance (ROE DIN 43582:1983/VDE 0303 part 3; IEC 60167

Thermal Properties
CTE, linear 20°C40 µm/m-°C 23-55°C (45x15x10 mm); ISO 11359
Melting Point178 °C Peak Temperature; ISO 3146, ISO 11357
Deflection Temperature at 0.46 MPa (66 psi)175 °C ISO 75
Deflection Temperature at 1.8 MPa (264 psi)160 °C ISO 75
Vicat Softening Point170 °C 50N; ISO 306
Vicat Softening Point175 °C 10N; ISO 306
Flammability, UL94HB 1.6 mm
Flammability, UL94HB 3.2 mm
Printer friendly version Printer friendly version


New MatWeb Services

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。