Degussa AG Vestamid® LX9104 Nylon 12
Subcategory: Nylon; Nylon 12; Polymer; Thermoplastic
Material Notes: Description: VESTAMID LX9104 is a halogen-free flame-retardant and flexible PA 12 compound of flammability class V-0 at0.8mm according to UL 94 and a LOI of 28%. Information provided by degussa.
No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
| Physical Properties | Original Value | Comments |
|
| Density | 1.12 g/cc | ISO 1183 |
Mechanical Properties |
|
| Tensile Strength, Yield | 27 MPa | ISO 527-2/1A |
| Elongation at Break | Min 50 % | ISO 527-2/1A |
| Elongation at Yield | 24 % | ISO 527-2/1A |
| Tensile Modulus | 0.75 GPa | ISO 527-1/2 |
| Charpy Impact Unnotched | NB | 23°C; ISO 179/1eU |
| Charpy Impact, Notched, Low Temp | 0.3 J/cm² | -30°C; ISO 179/1eA |
| Charpy Impact, Unnotched Low Temp | 15 J/cm² | -30°C, Partial Break; ISO 179/1eU |
| Charpy Impact, Notched | 0.6 J/cm² | 23°C; ISO 179/1eA |
|
Printer friendly version |

|