Physical Properties | Original Value | Comments |
|
Specific Gravity | 1.47 g/cc | ASTM D792 |
Linear Mold Shrinkage | 0.001 - 0.002 cm/cm | 3.20 mm; ASTM D955 |
Linear Mold Shrinkage | 0.006 - 0.007 cm/cm | 6.40 mm; ASTM D955 |
Mechanical Properties |
|
Tensile Strength, Yield | 154 MPa | ASTM D638 |
Elongation at Break | 3 % | ASTM D638 |
Flexural Modulus | 12.1 GPa | ASTM D790 |
Flexural Strength | 217 MPa | ASTM D790 |
Izod Impact, Notched | 0.88 J/cm | ASTM D256 |
Electrical Properties |
|
Surface Resistance | 1000 - 1e+008 ohm | ASTM D257 |
Thermal Properties |
|
CTE, linear 20°C | 60 µm/m-°C | TMA, -30°C to 30°C |
Deflection Temperature at 0.46 MPa (66 psi) | 206 °C | Unannealed (3.20 mm); ASTM D648 |
Flammability, UL94 | V-0 | 1.50 mm |
|