LNP (SABIC Innovative Plastics) VALOX® EXCP0212 Polybutylene Terephthalate, 45% Graphite Fiber Reinforcement
Subcategory: Filled/Reinforced Thermoplastic; Polybutylene Terephthalate (PBT); Polyester, TP; Polymer; Thermoplastic
Close Analogs: Saudi Basic Industries Corporation (SABIC) announced on August 31st, 2007, the completion of its purchase of GE Plastics.
Material Notes: Automotive heat sinks/spreaders, cooling fans. - Features: Thermally Conductive, Electrically Conductive, Flame Retardant
- Forms: Pellets
- Processing Method: Injection Molding
Information provided by LNP, a GE Plastics Company.
Physical Properties | Original Value | Comments |
|
Specific Gravity | 1.66 g/cc | ASTM D792 |
Mechanical Properties |
|
Tensile Strength at Break | 49 MPa | Type I, 5 mm/min; ASTM D638 |
Tensile Strength, Yield | 49 MPa | Type I, 5 mm/min; ASTM D638 |
Elongation at Break | 1.7 % | Type I, 5 mm/min; ASTM D638 |
Flexural Modulus | 8.64 GPa | (50.8 mm Span) 1mm/min; ASTM D790 |
Flexural Strength | 73.8 MPa | at Break, (50.8 mm Span) 1mm/min; ASTM D790 |
Izod Impact, Notched | 0.16 J/cm | ASTM D256 |
Izod Impact, Unnotched | 0.907 J/cm | ASTM D256 |
Falling Dart Impact | 4.34 J | ASTM D3763 |
Electrical Properties |
|
Volume Resistivity | 160 ohm-cm | ASTM D257 |
Surface Resistance | 100000 ohm | ASTM D257 |
Thermal Properties |
|
Thermal Conductivity | 1.1 W/m-K | ASTM C177 |
Deflection Temperature at 0.46 MPa (66 psi) | 213 °C | Unannealed (3.18 mm); ASTM D648 |
Deflection Temperature at 1.8 MPa (264 psi) | 161 °C | Unannealed (3.18 mm); ASTM D648 |
Processing Properties |
|
Rear Barrel Temperature | 238 - 254 °C | |
Middle Barrel Temperature | 243 - 260 °C | |
Front Barrel Temperature | 249 - 266 °C | |
Nozzle Temperature | 243 - 260 °C | |
Melt Temperature | 249 - 266 °C | |
Mold Temperature | 48.9 - 76.7 °C | |
Drying Temperature | 121 °C | |
Dry Time | 3 - 12 hour | |
Moisture Content | 0.02 % | Suggested |
Back Pressure | 0.345 - 0.689 MPa | |
Clamp Pressure | 41 - 69 MPa | |
Shot Size | 40 - 80 % | Suggested |
Vent Depth | 0.0025 - 0.0038 cm | |
Screw Speed | 50 - 100 rpm | |
|