LNP (SABIC Innovative Plastics) VALOX® EXCP0216 Polybutylene Terephthalate, 45% Carbon Fiber Reinforcement

Return to last searchReturn to last search
Printer friendly version Printer friendly versionAdd to Folder:
Excel Download Download to Excel (requires Excel and Windows)
 Export data to your CAD/FEA program

Subcategory: Filled/Reinforced Thermoplastic; Polybutylene Terephthalate (PBT); Polyester, TP; Polymer; Thermoplastic

Close Analogs: Saudi Basic Industries Corporation (SABIC) announced on August 31st, 2007, the completion of its purchase of GE Plastics.

Material Notes:
Automotive heat sinks/spreaders, cooling fans.

  • Features: Thermally Conductive, Electrically Conductive, Flame Retardant, High Strength
  • Forms: Pellets
  • Processing Method: Injection Molding
Information provided by LNP, a GE Plastics Company.

Physical PropertiesOriginal ValueComments
Specific Gravity1.66 g/cc ASTM D792

Mechanical Properties
Tensile Strength at Break88.9 MPa Type I, 5 mm/min; ASTM D638
Tensile Strength, Yield88.9 MPa Type I, 5 mm/min; ASTM D638
Elongation at Break1.5 % Type I, 5 mm/min; ASTM D638
Flexural Modulus22.9 GPa (50.8 mm Span) 1mm/min; ASTM D790
Flexural Strength128 MPa at Break, (50.8 mm Span) 1mm/min; ASTM D790
Izod Impact, Notched0.214 J/cm ASTM D256
Izod Impact, Unnotched1.33 J/cm ASTM D256
Falling Dart Impact5.2 J ASTM D3763

Electrical Properties
Volume Resistivity10 ohm-cm ASTM D257
Surface Resistance100000 ohm ASTM D257

Thermal Properties
Thermal Conductivity1.2 W/m-K ASTM C177
Deflection Temperature at 1.8 MPa (264 psi)189 °C Unannealed (3.18 mm); ASTM D648

Processing Properties
Rear Barrel Temperature238 - 254 °C 
Middle Barrel Temperature243 - 260 °C 
Front Barrel Temperature249 - 266 °C 
Nozzle Temperature243 - 260 °C 
Melt Temperature249 - 266 °C 
Mold Temperature48.9 - 76.7 °C 
Drying Temperature121 °C 
Dry Time3 - 12 hour 
Moisture Content0.02 % Suggested
Back Pressure0.345 - 0.689 MPa 
Clamp Pressure41 - 69 MPa 
Shot Size40 - 80 % Suggested
Vent Depth0.0025 - 0.0038 cm 
Screw Speed50 - 100 rpm 
Printer friendly version Printer friendly version


Instant Quotes for Quick Parts!Upload your 3D CAD model, select process, quantity, material, and instantly receive your unique, binding quote.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。