Specialty Compounds RTP Company

RTP Company RTP 1400 N Polyethersulfone (PES) High Viscosity

Return to last searchReturn to last search
Printer friendly version Printer friendly versionAdd to Folder:
Excel Download Download to Excel (requires Excel and Windows)Material suppliers Material suppliers
 Export data to your CAD/FEA program

Subcategory: Polyethersulfone; Polymer; Thermoplastic

Click here to view available vendors for this material.

Physical PropertiesOriginal ValueComments
Specific Gravity1.37 g/cc ASTM D792
Water Absorption0.54 % 24 hrs; 23°C; ASTM D570
Linear Mold Shrinkage0.006 cm/cm 1/8 in (3.2 mm); ASTM D955
Melt Flow30 g/10 min 385°C/2160 kg; ASTM D1238

Mechanical Properties
Tensile Strength @ Break12000 psi ASTM D638
Elongation at Break6.5 % ASTM D638
Tensile Modulus390000 psi ASTM D638
Flexural Modulus420000 psi ASTM D638
Flexural Yield Strength16100 psi ASTM D790
Izod Impact, Notched1.6 ft-lb/in 1/8 in (3.2 mm); ASTM D256

Electrical Properties
Volume ResistivityMin 1e+012 ohm-cm ASTM D257
Dielectric Constant3.5 1 MHz; Dry; ASTM D150
Dielectric Strength380 V/mil S/T; in oil; ASTM D149
Dissipation Factor0.0056 1 MHz; Dry; ASTM D150

Thermal Properties
CTE, linear 68°F27 µin/in-°F Flow Direction; ASTM E831
Deflection Temperature at 1.8 MPa (264 psi)400 °F ASTM D648
Flammability, UL94V-0 1/16 in (1.5 mm)

Processing Properties
Melt Temperature650 - 710 °F 
Mold Temperature275 - 350 °F 
Drying Temperature300 °F 6 hrs
Moisture Content0.04 % 
Dew Point-25 °F 
Injection Pressure10000 - 15000 psi 
Printer friendly version Printer friendly version


Specialty Compounds RTP Company

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。