MatWeb - Material Property Data 用 MatWeb 登广告!    Register Now
越过59,000 以上, 金属、塑料、陶瓷和合成物的数据资料库。
MatWeb - Material Property Data 主页  •  搜寻  •  工具  •  供应商  •  文件夹  •  有关我们  •  常用问题  •  登录   •  English English English 
  搜寻方法:  高级先进 | 材料类型 | 特性 | 构成份  | 商标  | 制造商
    Search

Specialty Compounds RTP Company

RTP Company ESD A 1480 Polyethersulfone (PES) Carbon Fiber - ESD Protection - Static Dissipative

Return to last searchReturn to last search
Printer friendly version Printer friendly versionAdd to Folder:
Excel Download Download to Excel (requires Excel and Windows)Material suppliers Material suppliers
 Export data to your CAD/FEA program

Subcategory: Polyethersulfone; Polymer; Thermoplastic

Click here to view available vendors for this material.

Physical PropertiesOriginal ValueComments
Specific Gravity1.38 g/cc ASTM D792
Linear Mold Shrinkage0.003 cm/cm 1/8 in (3.2 mm); ASTM D955

Mechanical Properties
Tensile Strength @ Break17000 psi ASTM D638
Elongation at Break2 - 3 % ASTM D638
Tensile Modulus1e+006 psi ASTM D638
Flexural Modulus1e+006 psi ASTM D638
Flexural Yield Strength25000 psi ASTM D790
Izod Impact, Unnotched9 ft-lb/in 1/8 in (3.2 mm); ASTM D4812
Izod Impact, Notched1 ft-lb/in 1/8 in (3.2 mm); ASTM D256

Electrical Properties
Volume Resistivity1000 - 9.9e+009 ohm-cm ASTM D257
Surface Resistance10000 - 9.9e+011 ohm ESD S11.11
Surface Resistivity per Square100000 - 9.9e+012 ohm ASTM D257; ESD S11.11
Static DecayMax 2 sec FTMS101C; 4046.1

Processing Properties
Melt Temperature650 - 710 °F 
Mold Temperature275 - 350 °F 
Drying Temperature300 °F 6 hrs
Moisture Content0.04 % 
Dew Point-25 °F 
Injection Pressure10000 - 15000 psi 
Printer friendly version Printer friendly version


Specialty Compounds RTP Company

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。