RTP Company RTP 1400 GB 20 Polyethersulfone (PES) Glass Bead 20%
Subcategory: Polyethersulfone; Polymer; Thermoplastic
Close Analogs: Data for this product has not been recently verified, please contact RTP Company for more information before specifying this grade.
Material Notes: Glass Bead 20% Comments: Unless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties. Information provided by RTP Company.
Click here to view available vendors for this material.
| Physical Properties | Original Value | Comments |
|
| Specific Gravity | 1.51 g/cc | ASTM D792 |
| Water Absorption | 0.4 % | 24 hours at 23°C; ASTM D570 |
| Linear Mold Shrinkage | 0.007 cm/cm | 1/8 inch (3.18 mm) section; ASTM D955 |
| Linear Mold Shrinkage, 6.35 mm section | 0.008 cm/cm | 1/4 inch (6.35 mm) section; ASTM D955 |
Mechanical Properties |
|
| Hardness, Rockwell R | 125 | ASTM D785 |
| Tensile Strength, Ultimate | 11800 psi | ASTM D638 |
| Elongation at Break | 3.1 % | ASTM D638 |
| Modulus of Elasticity | 650 ksi | ASTM D638 |
| Flexural Modulus | 550 ksi | ASTM D790 |
| Flexural Yield Strength | 20000 psi | ASTM D790 |
| Izod Impact, Unnotched | 3.5 ft-lb/in | 1/8 in (3.18 mm) section; ASTM D256 |
| Izod Impact, Notched | 0.6 ft-lb/in | 1/8 in (3.18 mm) section; ASTM D256 |
Electrical Properties |
|
| Electrical Resistivity | 1e+016 ohm-cm | ASTM D257 |
Thermal Properties |
|
| Deflection Temperature at 1.8 MPa (264 psi) | 400 °F | ASTM D648 |
| Flammability, UL94 | V-0 | (V-0) at 1/16 in (1.59 mm); Per testing by RTP Company; ASTM D3801 |
Processing Properties |
|
| Processing Temperature | 650 - 690 °F | |
| Mold Temperature | 275 - 350 °F | |
| Injection Pressure | 10000 - 15000 psi | |
Descriptive Properties | |
| Color | Natural/Black | |
|