RTP Company RTP 1405 HF TFE 15 Polyethersulfone (PES) Glass Fiber 30% - PTFE 15% - High Flow
Subcategory: Polyethersulfone; Polymer; Thermoplastic
Close Analogs: Data for this product has not been recently verified, please contact RTP Company for more information before specifying this grade.
Material Notes: Glass Fiber 30% - PTFE 15% - High Flow Comments: - Glass Fiber
- PTFE Lubricated
- High Flow
Unless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties. Information provided by RTP Company.
Click here to view available vendors for this material.
Physical Properties | Original Value | Comments |
|
Specific Gravity | 1.69 g/cc | ASTM D792 |
Filler Content | 30 % | |
Linear Mold Shrinkage | 0.005 cm/cm | 1/8 inch (3.18 mm) section; ASTM D955 |
Mechanical Properties |
|
Tensile Strength, Ultimate | 16000 psi | ASTM D638 |
Elongation at Break | 1.4 % | ASTM D638 |
Modulus of Elasticity | 1500 ksi | ASTM D638 |
Flexural Modulus | 1300 ksi | ASTM D790 |
Flexural Yield Strength | 25000 psi | ASTM D790 |
Izod Impact, Unnotched | 9 ft-lb/in | 1/8 in (3.18 mm) section; ASTM D256 |
Izod Impact, Notched | 2 ft-lb/in | 1/8 in (3.18 mm) section; ASTM D256 |
Thermal Properties |
|
Deflection Temperature at 1.8 MPa (264 psi) | 400 °F | ASTM D648 |
Processing Properties |
|
Processing Temperature | 650 - 690 °F | |
Mold Temperature | 275 - 350 °F | |
Injection Pressure | 10000 - 15000 psi | |
Descriptive Properties | |
Color | Natural/Black | |
|
Printer friendly version |
|