RTP Company RTP 1405 N L Polyethersulfone (PES) Glass Fiber 30% - Lubricated - High Viscosity
Subcategory: Polyethersulfone; Polymer; Thermoplastic
Close Analogs: Data for this product has not been recently verified, please contact RTP Company for more information before specifying this grade.
Material Notes: Glass Fiber 30% - Lubricated - High Viscosity Comments: - Glass Fiber
- Lubricated
- High Viscosity
Unless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties. Information provided by RTP Company.
Click here to view available vendors for this material.
| Physical Properties | Original Value | Comments |
|
| Specific Gravity | 1.59 g/cc | ASTM D792 |
| Filler Content | 30 % | |
| Water Absorption | 0.35 % | 24 hours at 23°C; ASTM D570 |
| Linear Mold Shrinkage | 0.002 cm/cm | 1/8 inch (3.18 mm) section; ASTM D955 |
| Linear Mold Shrinkage, 6.35 mm section | 0.002 cm/cm | 1/4 inch (6.35 mm) section; ASTM D955 |
Mechanical Properties |
|
| Hardness, Rockwell R | 123 | ASTM D785 |
| Tensile Strength, Ultimate | 21500 psi | ASTM D638 |
| Elongation at Break | 2.6 % | ASTM D638 |
| Modulus of Elasticity | 1400 ksi | ASTM D638 |
| Flexural Modulus | 1300 ksi | ASTM D790 |
| Flexural Yield Strength | 30500 psi | ASTM D790 |
| Compressive Yield Strength | 21000 psi | ASTM D695 |
| Izod Impact, Unnotched | 14 ft-lb/in | 1/8 in (3.18 mm) section; ASTM D256 |
| Izod Impact, Notched | 1.8 ft-lb/in | 1/8 in (3.18 mm) section; ASTM D256 |
Electrical Properties |
|
| Electrical Resistivity | 1e+016 ohm-cm | ASTM D257 |
| Dielectric Constant | 4.2 | 1 MHz, Dry; ASTM D150 |
| Dielectric Strength | 370 V/mil | S/T; ASTM D149 |
| Dissipation Factor | 0.007 | 1 MHz, Dry; ASTM D150 |
| Arc Resistance | 75 sec | ASTM D495 |
Thermal Properties |
|
| CTE, linear 68°F | 15 µin/in-°F | Flow Direction; ASTM D696 |
| Thermal Conductivity | 2.2 BTU-in/hr-ft²-°F | Through-plane; ASTM C177 |
| Deflection Temperature at 0.46 MPa (66 psi) | 430 °F | ASTM D648 |
| Deflection Temperature at 1.8 MPa (264 psi) | 415 °F | ASTM D648 |
| Flammability, UL94 | V-0 | (V-0) at 1/16 in (1.59 mm); Per testing by RTP Company; ASTM D3801 |
Processing Properties |
|
| Processing Temperature | 650 - 690 °F | |
| Mold Temperature | 275 - 350 °F | |
| Injection Pressure | 10000 - 15000 psi | |
Descriptive Properties | |
| Color | Natural/Black | |
|
Printer friendly version |

|