RTP Company RTP 1400 R-4300 UV Polyethersulfone (PES) PC Alloy - UV Stable
Subcategory: Polyethersulfone; Polymer; Thermoplastic
Close Analogs: Data for this product has not been recently verified, please contact RTP Company for more information before specifying this grade.
Material Notes: PC Alloy - UV Stable Comments: Unless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties. Information provided by RTP Company.
Click here to view available vendors for this material.
Physical Properties | Original Value | Comments |
|
Specific Gravity | 1.32 g/cc | ASTM D792 |
Linear Mold Shrinkage | 0.0065 cm/cm | 1/8 inch (3.18 mm) section; ASTM D955 |
Mechanical Properties |
|
Tensile Strength, Ultimate | 11100 psi | ASTM D638 |
Elongation at Break | Min 10 % | ASTM D638 |
Modulus of Elasticity | 380 ksi | ASTM D638 |
Flexural Modulus | 380 ksi | ASTM D790 |
Flexural Yield Strength | 16500 psi | ASTM D790 |
Izod Impact, Unnotched | 34 ft-lb/in | 1/8 in (3.18 mm) section; ASTM D256 |
Izod Impact, Notched | 4 ft-lb/in | 1/8 in (3.18 mm) section; ASTM D256 |
Electrical Properties |
|
Electrical Resistivity | 1e+015 ohm-cm | ASTM D257 |
Thermal Properties |
|
Deflection Temperature at 1.8 MPa (264 psi) | 360 °F | ASTM D648 |
Processing Properties |
|
Processing Temperature | 650 - 690 °F | |
Mold Temperature | 275 - 350 °F | |
Injection Pressure | 10000 - 15000 psi | |