RTP Company ESD C 1480 N Polyethersulfone (PES) Conductive - Carbon Fiber - High Viscosity
Subcategory: Polyethersulfone; Polymer; Thermoplastic
Close Analogs: Data for this product has not been recently verified, please contact RTP Company for more information before specifying this grade.
Material Notes: Conductive - Carbon Fiber - High Viscosity Comments: - Conductive
- ESD Protection
- Carbon Fiber
- High Viscosity
Unless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties. Information provided by RTP Company.
Click here to view available vendors for this material.
| Physical Properties | Original Value | Comments |
|
| Specific Gravity | 1.39 g/cc | ASTM D792 |
| Water Absorption | 0.4 % | 24 hours at 23°C; ASTM D570 |
| Linear Mold Shrinkage | 0.002 cm/cm | 1/8 inch (3.18 mm) section; ASTM D955 |
| Linear Mold Shrinkage, 6.35 mm section | 0.004 cm/cm | 1/4 inch (6.35 mm) section; ASTM D955 |
Mechanical Properties |
|
| Tensile Strength, Ultimate | 15000 psi | ASTM D638 |
| Elongation at Break | 3 - 4 % | ASTM D638 |
| Modulus of Elasticity | 850 ksi | ASTM D638 |
| Flexural Modulus | 750 ksi | ASTM D790 |
| Flexural Yield Strength | 24000 psi | ASTM D790 |
| Izod Impact, Unnotched | 10 ft-lb/in | 1/8 in (3.18 mm) section; ASTM D256 |
| Izod Impact, Notched | 1 ft-lb/in | 1/8 in (3.18 mm) section; ASTM D256 |
Electrical Properties |
|
| Electrical Resistivity | 1000 - 1e+009 ohm-cm | ASTM D257 |
| Surface Resistance | 1e+006 - 1e+012 ohm | ASTM D257 |
| Static Decay | Max 2 sec | FTMS-4046.1 |
Thermal Properties |
|
| Deflection Temperature at 0.46 MPa (66 psi) | 405 °F | ASTM D648 |
| Deflection Temperature at 1.8 MPa (264 psi) | 400 °F | ASTM D648 |
| Flammability, UL94 | V-0 | (V-0) at 0.06 in (1.5 mm); Per testing by RTP Company; ASTM D3801 |
Processing Properties |
|
| Processing Temperature | 650 - 690 °F | |
| Mold Temperature | 275 - 350 °F | |
| Injection Pressure | 10000 - 15000 psi | |
Descriptive Properties | |
| Color | Natural/Black | |
|