BASF Elastollan® C-80A Polyester Type Polyurethane Elastomer

Return to last searchReturn to last search
Printer friendly version Printer friendly versionAdd to Folder:
Excel Download Download to Excel (requires Excel and Windows)Material suppliers Material suppliers
 Export data to your CAD/FEA program

Subcategory: Elastomer, TPE; Polymer; Polyurethane, TP; Thermoplastic

Key Words: TPU Rubbers

Material Notes:
Processed by extrusion or injection molding. Elastollan C series of products are polyester-based thermoplastic polyurethanes that exhibit very good hydrolytic stability. They also exhibit excellent oil, fuel and solvent resistance. These products can be injection and blow molded and extruded.

As with all TPU products this grade must be dried prior to processing.

Property values below are typical values based on test samples cured 20 hours at 100°C before testing. Information provided by BASF Corporation.

Click here to view available vendors for this material.

Physical PropertiesOriginal ValueComments
Density1.19 g/cc ASTM D792

Mechanical Properties
Hardness, Shore A82 ASTM D2240
Tensile Strength, Ultimate36 MPa ASTM D412
Tensile Strength, Yield1.1 MPa Tensile stress at 300% elongation.; ASTM D-412
Tensile Strength, Yield5.5 MPa Tensile stress at 100% elongation.; ASTM D-412
Elongation at Break700 % ASTM D412
Tear Strength85 kN/m ASTM D624
Taber Abrasion, mg/1000 Cycles25 H-18 wheel; ASTM D-1044.
Tensile Set30 % at break; ASTM D-412

Electrical Properties
Electrical ResistivityMin 1e+010 ohm-cm DIN 53482/VDE 0303
Surface ResistanceMin 1e+010 ohm DIN 53482/VDE 0303
Dielectric Constant6.1 1 MHz; DIN 53483/VDE 0303
Dielectric Constant6.6 1 kHz; DIN 53483/VDE 0303
Dielectric Constant, Low Frequency7.1 at 50 Hz; DIN 53483/VDE 0303
Dielectric Strength31 kV/mm DIN 53481/VDE 0303
Dissipation Factor0.024 1 kHz
Dissipation Factor0.053 1 MHz
Dissipation Factor, Low Frequency0.2 50 Hz
Comparative Tracking IndexMin 600 V DIN/IRC 112
Printer friendly version Printer friendly version


Instant Quotes for Quick Parts!Upload your 3D CAD model, select process, quantity, material, and instantly receive your unique, binding quote.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。