BASF Elastollan® C-85A Polyester Type Polyurethane Elastomer
Subcategory: Elastomer, TPE; Polymer; Polyurethane, TP; Thermoplastic
Key Words: TPU Rubbers
Material Notes: Processed by extrusion or injection molding. Elastollan C series of products are polyester-based thermoplastic polyurethanes that exhibit very good hydrolytic stability. They also exhibit excellent oil, fuel and solvent resistance. These products can be injection and blow molded and extruded. As with all TPU products this grade must be dried prior to processing. Property values below are typical values based on test samples cured 20 hours at 100°C before testing. Information provided by BASF Corporation.
Click here to view available vendors for this material.
Physical Properties | Original Value | Comments |
|
Density | 1.19 g/cc | ASTM D792 |
Mechanical Properties |
|
Hardness, Shore A | 85 | ASTM D2240 |
Tensile Strength, Ultimate | 39 MPa | ASTM D412 |
Tensile Strength, Yield | 1.3 MPa | Tensile stress at 300% elongation.; ASTM D-412 |
Tensile Strength, Yield | 6.6 MPa | Tensile stress at 100% elongation.; ASTM D-412 |
Elongation at Break | 620 % | ASTM D412 |
Modulus of Elasticity | 0.02 GPa | |
Shear Modulus | 0.012 GPa | |
Tear Strength | 95 kN/m | ASTM D624 |
Taber Abrasion, mg/1000 Cycles | 25 | H-18 wheel; ASTM D-1044. |
Tensile Set | 35 % | at break; ASTM D-412 |
Electrical Properties |
|
Comparative Tracking Index | Min 600 V | DIN/IRC 112 |
Thermal Properties |
|
Vicat Softening Point | 95 °C | |
Flammability, UL94 | HB | Color: NC. 0.95 mm. |
|
Printer friendly version |
|