BASF Elastollan® C-95A Polyester Type Polyurethane Elastomer
Subcategory: Elastomer, TPE; Polymer; Polyurethane, TP; Thermoplastic
Key Words: TPU Rubbers
Material Notes: Processed by extrusion or injection molding. Elastollan C series of products are polyester-based thermoplastic polyurethanes that exhibit very good hydrolytic stability. They also exhibit excellent oil, fuel and solvent resistance. These products can be injection and blow molded and extruded. As with all TPU products this grade must be dried prior to processing. Property values below are typical values based on test samples cured 20 hours at 100°C before testing. Information provided by BASF Corporation.
Click here to view available vendors for this material.
| Physical Properties | Original Value | Comments |
|
| Density | 1.21 g/cc | ASTM D792 |
Mechanical Properties |
|
| Hardness, Shore A | 96 | ASTM D2240 |
| Hardness, Shore D | 46 | ASTM D2240 |
| Tensile Strength, Ultimate | 40 MPa | ASTM D412 |
| Tensile Strength, Yield | 13 MPa | Tensile stress at 100% elongation.; ASTM D-412 |
| Tensile Strength, Yield | 26 MPa | Tensile stress at 300% elongation.; ASTM D-412 |
| Elongation at Break | 480 % | ASTM D412 |
| Modulus of Elasticity | 0.15 GPa | |
| Shear Modulus | 0.045 GPa | |
| Tear Strength | 140 kN/m | ASTM D624 |
| Taber Abrasion, mg/1000 Cycles | 35 | H-18 wheel; ASTM D-1044. |
| Tensile Set | 65 % | at break; ASTM D-412 |
Electrical Properties |
|
| Electrical Resistivity | Min 1e+011 ohm-cm | DIN 53482/VDE 0303 |
| Surface Resistance | Min 1e+011 ohm | DIN 53482/VDE 0303 |
| Dielectric Constant | 5.3 | 1 MHz; DIN 53483/VDE 0303 |
| Dielectric Constant | 6.1 | 1 kHz; DIN 53483/VDE 0303 |
| Dielectric Constant, Low Frequency | 6.4 | at 50 Hz; DIN 53483/VDE 0303 |
| Dielectric Strength | 48 kV/mm | DIN 53481/VDE 0303 |
| Dissipation Factor | 0.024 | 1 kHz |
| Dissipation Factor | 0.054 | 1 MHz |
| Dissipation Factor, Low Frequency | 0.036 | 50 Hz |
| Comparative Tracking Index | Min 600 V | DIN/IRC 112 |
Thermal Properties |
|
| Vicat Softening Point | 145 °C | |
|
Printer friendly version |
|