BASF Elastollan® 1185A Polyether Type Polyurethane Elastomer
Subcategory: Elastomer, TPE; Polymer; Polyurethane, TP; Thermoplastic
Key Words: TPU Rubbers
Material Notes: Processed by extrusion or injection molding. Elastollan ® 1100 series products are FDA Sec. 177.2600 compliant. Elastollan 1100 series of products are polyether-based thermoplastic polyurethanes. They exhibit excellent low temperature properties, hydrolysis resistance and fungus resistance. These products can be injection and blow molded and extruded. As with all TPU products this grade must be dried prior to processing. Property values below are typical values based on test samples cured 20 hours at 100°C before testing. Information provided by BASF Corporation.
Click here to view available vendors for this material.
Physical Properties | Original Value | Comments |
|
Density | 1.12 g/cc | ASTM D792 |
Mechanical Properties |
|
Hardness, Shore A | 86 | ASTM D2240 |
Tensile Strength, Ultimate | 33 MPa | ASTM D412 |
Tensile Strength, Yield | 12 MPa | Tensile stress at 300% elongation.; ASTM D-412 |
Tensile Strength, Yield | 7.6 MPa | Tensile stress at 100% elongation.; ASTM D-412 |
Elongation at Break | 640 % | ASTM D412 |
Modulus of Elasticity | 0.025 GPa | |
Poisson's Ratio | 0.25 | Calculated |
Shear Modulus | 0.01 GPa | |
Tear Strength | 105 kN/m | ASTM D624 |
Taber Abrasion, mg/1000 Cycles | 30 | H-18 wheel; ASTM D-1044. |
Tensile Set | 70 % | at break; ASTM D-412 |
Electrical Properties |
|
Comparative Tracking Index | Min 600 V | DIN/IRC 112 |
Thermal Properties |
|
Vicat Softening Point | 85 °C | |
|