BASF Elastollan® 1174D Polyether Type Polyurethane Elastomer
Subcategory: Elastomer, TPE; Polymer; Polyurethane, TP; Thermoplastic
Key Words: TPU Rubbers
Material Notes: Recommended for injection molding. Elastollan ® 1100 series products are FDA Sec. 177.2600 compliant. Elastollan 1100 series of products are polyether-based thermoplastic polyurethanes. They exhibit excellent low temperature properties, hydrolysis resistance and fungus resistance. These products can be injection and blow molded and extruded. As with all TPU products this grade must be dried prior to processing. Property values below are typical values based on test samples cured 20 hours at 100°C before testing. Information provided by BASF Corporation.
Click here to view available vendors for this material.
Physical Properties | Original Value | Comments |
|
Density | 1.19 g/cc | ASTM D792 |
Mechanical Properties |
|
Hardness, Shore D | 73 | ASTM D2240 |
Tensile Strength, Ultimate | 45 MPa | ASTM D412 |
Tensile Strength, Yield | 32 MPa | Tensile stress at 100% elongation.; ASTM D-412 |
Tensile Strength, Yield | 38 MPa | Tensile stress at 300% elongation.; ASTM D-412 |
Elongation at Break | 350 % | ASTM D412 |
Tear Strength | 255 kN/m | ASTM D624 |
Taber Abrasion, mg/1000 Cycles | 75 | H-18 wheel; ASTM D-1044. |
Tensile Set | 80 % | at break; ASTM D-412 |
Electrical Properties |
|
Electrical Resistivity | Min 1e+012 ohm-cm | DIN 53482/VDE 0303 |
Surface Resistance | Min 1e+012 ohm | DIN 53482/VDE 0303 |
|