BASF Elastollan® 1185A10X Wire & Cable Grade Polyurethane Elastomer
Subcategory: Elastomer, TPE; Polymer; Polyurethane, TP; Thermoplastic
Key Words: TPU Rubbers
Material Notes: Compliant with NSF Standard 61 (Drinking water contact). As with all TPU products this grade must be dried prior to processing. Information provided by BASF Corporation.
Click here to view available vendors for this material.
| Physical Properties | Original Value | Comments |
|
| Density | 1.12 g/cc | 2.0 mm (0.080 in) molded plaque, cured 20 hr at 100°C.; ASTM D792 |
Mechanical Properties |
|
| Hardness, Shore A | 86 | 2.0 mm (0.080 in) molded plaque, cured 20 hr at 100°C.; ASTM D2240 |
| Tensile Strength, Ultimate | 52 MPa | 2.0 mm (0.080 in) molded plaque, cured 20 hr at 100°C; ASTM D412 |
| Tensile Strength, Yield | 19 MPa | Tensile stress at 300% elongation; 0.76 mm (0.030 in) extruded sheet; ASTM D-412 |
| Tensile Strength, Yield | 7.6 MPa | Tensile stress at 100% elongation.; ASTM D-412 |
| Elongation at Break | 570 % | on 0.030 in extruded sheet; ASTM D-412 |
| Flexural Modulus | 0.043 GPa | 2.0 mm (0.080 in) molded plaque, cured 20 hr at 100°C.; ASTM D790 |
| Tear Strength | 66 kN/m | Split tear strength (ASTM D-1938) on 0.76 mm ( 0.030 inch) extruded sheet |
| Graves Tear Strength | 88 kN/m | on 0.76 mm ( 0.030 inch) extruded sheet; ASTM D624 |
| Taber Abrasion, mg/1000 Cycles | 25 | H-18 wheel; ASTM D-1044; 2.0 mm (0.080 in) molded plaque, cured 20 hr at 100°C. |
| Compression Set | 25 % | 22 hr at 23°C per ASTM D-395; 2.0 mm (0.080 in) molded plaque, cured 20 hr at 100°C. |
| Compression Set, Elevated Temperature | 45 % | 22 hr @ 70°C; ASTM D-395; 0.080 in molded plaque after curing 20 hrs at 100°C. |
| Tensile Set | 32 % | at 200% elongation per ASTM D-412 is on 0.030 in extruded sheet. |
Thermal Properties |
|
| Vicat Softening Point | 100 °C | 2.0 mm (0.080 in) molded plaque, cured 20 hr at 100°C.; ASTM D1525 |
| Glass Temperature | -40 °C | Pellet sample |
|
Printer friendly version |
|