BASF Elastollan® 1190A10 Wire & Cable Grade Polyurethane Elastomer
Subcategory: Elastomer, TPE; Polymer; Polyurethane, TP; Thermoplastic
Key Words: TPU Rubbers
Material Notes: As with all TPU products this grade must be dried prior to processing. Information provided by BASF Corporation.
Click here to view available vendors for this material.
| Physical Properties | Original Value | Comments |
|
| Density | 1.13 g/cc | 2.0 mm (0.080 in) molded plaque, cured 20 hr at 100°C.; ASTM D792 |
Mechanical Properties |
|
| Hardness, Shore A | 90 | 2.0 mm (0.080 in) molded plaque, cured 20 hr at 100°C.; ASTM D2240 |
| Tensile Strength, Ultimate | 55 MPa | 2.0 mm (0.080 in) molded plaque, cured 20 hr at 100°C; ASTM D412 |
| Tensile Strength, Yield | 25 MPa | Tensile stress at 300% elongation; 0.76 mm (0.030 in) extruded sheet; ASTM D-412 |
| Tensile Strength, Yield | 9 MPa | Tensile stress at 100% elongation.; ASTM D-412 |
| Elongation at Break | 500 % | on 0.030 in extruded sheet; ASTM D-412 |
| Flexural Modulus | 0.05 GPa | 2.0 mm (0.080 in) molded plaque, cured 20 hr at 100°C.; ASTM D790 |
| Tear Strength | 58 kN/m | Split tear strength (ASTM D-1938) on 0.76 mm ( 0.030 inch) extruded sheet |
| Graves Tear Strength | 114 kN/m | on 0.76 mm ( 0.030 inch) extruded sheet; ASTM D624 |
| Taber Abrasion, mg/1000 Cycles | 30 | H-18 wheel; ASTM D-1044; 2.0 mm (0.080 in) molded plaque, cured 20 hr at 100°C. |
| Compression Set | 25 % | 22 hr at 23°C per ASTM D-395; 2.0 mm (0.080 in) molded plaque, cured 20 hr at 100°C. |
| Compression Set, Elevated Temperature | 45 % | 22 hr @ 70°C; ASTM D-395; 0.080 in molded plaque after curing 20 hrs at 100°C. |
| Tensile Set | 32 % | at 200% elongation per ASTM D-412 is on 0.030 in extruded sheet. |
Thermal Properties |
|
| Vicat Softening Point | 110 °C | 2.0 mm (0.080 in) molded plaque, cured 20 hr at 100°C.; ASTM D1525 |
| Glass Temperature | -35 °C | Pellet sample |
|