Aluminum, Al
Subcategory: Aluminum Alloy; Pure Element; Nonferrous Metal
Close Analogs: Over 1175 Al alloys are listed in MatWeb. Aluminum 1199 is the highest purity (99.99% Al min.) commercially available in structural form.
Material Notes: This listing is for pure aluminum.