Gold, Au
Subcategory: Pure Element; Precious Metal; Nonferrous Metal; Gold Alloy
Material Notes: Gold is a noble metal and does not react with oxygen. This is why gold does not tarnish. Although it does not form oxides, it will form compounds with other metals and is rarely found in its pure form. It is usually associated with silver and often with mercury. When the silver content is a high, the metal is called electrum, a naturally occurring gold-silver alloy. Gold is also found in tellurides and ore containing quartz where it is either openly visible or enclosed in particles of sulfide minerals such as chalcopyrite, pyrrhotite, pyrite, and arsenopyrite. Gold in its pure form is a very soft metal, so it is often alloyed with other metals for increased strength and hardness. When gold is alloyed, its ductility is diminished, but its malleability remains constant, except when large amounts of copper are added. Red or pink gold (also called rose gold) is gold that contains large percentages of copper and a small amount of silver. Green gold is usually gold alloyed with additional silver or with silver that has a small percentage of copper. White gold is usually 75% gold and 25% nickel (or nickel, zinc, and sometimes copper). Formally white gold was made with silver and/or palladium, but white gold made with nickel and zinc is harder, cheaper, and has better melting characteristics.
| Available Properties |
- Density
- Hardness, Vickers
- Tensile Strength, Ultimate
- Elongation at Break
- Modulus of Elasticity
- Poissons Ratio
- Shear Modulus
- Electrical Resistivity
- Magnetic Susceptibility
- Heat of Fusion
- CTE, linear 20°C
- CTE, linear 250°C
- CTE, linear 500°C
- CTE, linear 1000°C
- Specific Heat Capacity
- Thermal Conductivity
- Melting Point
- Emissivity (0-1)
- Reflection Coefficient, Visible (0-1)
- CAS Number
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|