Copper, Cu; Annealed
Subcategory: Copper Alloy; Pure Element; Nonferrous Metal
Close Analogs: Over 2000 Cu alloy entries are listed in MatWeb.
Material Notes: Annealed applies only to tensile and/or hardness values; other property values are typical of the element. This entry is for pure Cu, MatWeb also has entries for many alloys.
| Available Properties |
- Density
- Hardness, Vickers
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Modulus of Elasticity
- Bulk Modulus
- Poissons Ratio
- Shear Modulus
- Electrical Resistivity
- Magnetic Susceptibility
- Heat of Fusion
- CTE, linear 20°C
- CTE, linear 250°C
- CTE, linear 500°C
- CTE, linear 1000°C
- Specific Heat Capacity
- Thermal Conductivity
- Melting Point
- Emissivity (0-1)
- Reflection Coefficient, Visible (0-1)
- CAS Number
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|