Molybdenum, Mo, Annealed
Subcategory: Pure Element; Nonferrous Metal; Molybdenum Alloy
Material Notes: Physical Form: Gray-Black Metal; Cubic. Annealed applies only to tensile and hardness values; other property values are typical of the element.
| Available Properties |
- Density
- Molecular Weight
- Hardness, Brinell
- Hardness, Rockwell A
- Hardness, Rockwell B
- Hardness, Rockwell C
- Hardness, Vickers
- Tensile Strength, Ultimate
- Modulus of Elasticity
- Compressive Yield Strength
- Bulk Modulus
- Shear Modulus
- Shear Strength
- Electrical Resistivity
- Magnetic Susceptibility
- Critical Magnetic Field Strength, Oersted
- Critical Superconducting Temperature
- Heat of Fusion
- CTE, linear 20°C
- CTE, linear 250°C
- CTE, linear 500°C
- CTE, linear 1000°C
- Specific Heat Capacity
- Thermal Conductivity
- Melting Point
- Boiling Point
- Heat of Formation
- Emissivity (0-1)
- Reflection Coefficient, Visible (0-1)
- CAS Number
- Solubility
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|