Osmium, Os; Arc-Melted
Subcategory: Pure Element; Precious Metal; Nonferrous Metal
Close Analogs: See entries for annealed and cold worked Os.
Material Notes: Arc-melted applies only to tensile and/or hardness values; other property values are typical of the element.Physical Form: Blue-White Metal; Hexagonal
| Available Properties |
- Density
- Molecular Weight
- Hardness, Brinell
- Hardness, Knoop
- Hardness, Rockwell A
- Hardness, Rockwell C
- Hardness, Vickers
- Modulus of Elasticity
- Electrical Resistivity
- Magnetic Susceptibility
- Critical Magnetic Field Strength, Oersted
- Critical Superconducting Temperature
- Heat of Fusion
- CTE, linear 20°C
- Specific Heat Capacity
- Thermal Conductivity
- Melting Point
- Boiling Point
- Heat of Formation
- Solubility
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|